Reflow Soldering (Beta Layout kit)
From Tech
Jump to navigationJump to searchConnecting to the Beta Layout Flow controller simply with screen:
screen -L /dev/ttyUSB0
The '-L' argument saves the session to a logfile. If screen exits without error, you may need to be root
Settings for Pb soldering:
phttemp 125 Preheat temperature: [0..254] degC phttime 150 Preheat time: [0..65534] Sekunden phtpwr 60 Preheat power: [0..100] % soaktemp 180 Soak temperature: [0..254] degC soaktime 90 Soak time: [0..65534] Sekunden soakpwr 80 Soak power: [0..100] % reflowtemp 230 Reflow temperature: [0..254] degC reflowtime 140 Reflow time: [0..65534] Sekunden reflowpwr 100 Reflow power: [0..100] % dwelltemp 232 Dwell temperature: [0..254] degC dwelltime 40 Dwell time: [0..65534] Sekunden dwellpwr 80 Dwell power: [0..100] % tempoffset- 10 temperature adjust [-30..30] deg debug OFF output debug information [0 or 1] trace OFF output internal status information [0 or 1] settings 0 select the active parameter set [0..4]
Settings for Sn96.5Ag3Cu0.5 soldering
- Same, but reflowtemp=245;
Boards (tested with PCBway boards) do start to smell, and the areas without copper turn darker (not black yet)